汽车用齿轮钢16MnCrS5热处理变形机理
屈小波, 安金敏, 王林, 李喜

Quenching Deformation of the 16MnCrS5 Gear Steel for Automobile
QU Xiaobo, AN Jinmin, WANG Lin, LI Xi
图8 16MnCrS5齿轮钢经热轧处理后以不同方式冷却获得的带状组织形貌的OM像
Fig.8 OM images showing the banded structure morphologies of the 16MnCrS5 samples after hot rolling with water-colling (a), air-cooling (b), and furnace cooling (c)