Hf和Ta对镍基粉末高温合金蠕变断裂特征和性能的影响 |
| 张浩鹏, 白佳铭, 李新宇, 李晓鲲, 贾建, 刘建涛, 张义文 |
|
Effect of Hf and Ta on Creep Rupture Characteristics and Properties of Powder Metallurgy Ni-Based Superalloys |
| ZHANG Haopeng, BAI Jiaming, LI Xinyu, LI Xiaokun, JIA Jian, LIU Jiantao, ZHANG Yiwen |
| 图9 Hf和Ta对热处理态合金中退火孪晶界密度的影响 |