Ag替换CuZr-Ti-Cu-Al非晶合金性能的影响
蔡正清, 尹大伟, 杨靓, 王文祥, 王飞龙, 温永清, 马明臻

Effect of Ag Substitution of Cu on Properties of Zr-Ti-Cu-Al Amorphous Alloys
CAI Zhengqing, YIN Dawei, YANG Liang, WANG Wenxiang, WANG Feilong, WEN Yongqing, MA Mingzhen
表1 Zr55Ti3Cu32 - x Al10Ag x 非晶合金的热物性参数和临界尺寸
Table 1 Thermal properties and Dcof the Zr55Ti3Cu32 - x Al10-Ag x BMGs
xTgTxTmTlTrgDc
KKKKmm
0673.0730.41133.81165.40.5774
1667.2729.71130.91164.30.5733
1.5673.8727.21127.61164.20.5796
2665.1726.41124.91161.10.5735
2.5665.0726.31123.41161.00.5735