Ag替换CuZr-Ti-Cu-Al非晶合金性能的影响
蔡正清, 尹大伟, 杨靓, 王文祥, 王飞龙, 温永清, 马明臻

Effect of Ag Substitution of Cu on Properties of Zr-Ti-Cu-Al Amorphous Alloys
CAI Zhengqing, YIN Dawei, YANG Liang, WANG Wenxiang, WANG Feilong, WEN Yongqing, MA Mingzhen
图9 Zr55Ti3Cu32 - x Al10Ag x 非晶合金腐蚀表面的SEM像
Fig.9 SEM images of Zr55Ti3Cu32 - x Al10Ag x BMG corroded surfaces in two kinds of solutions
(a) x = 0, PBS (b) x = 1.5, PBS (c) x = 0, SBF (d) x = 2, SBF