定向凝固与固态相变双联协控下Monel K-500合金的组织和力学性能 |
| 杨明辉, 李星吾, 孙崇昊, 阮莹 |
|
Microstructure and Mechanical Properties of Monel K-500 Alloy in Synergetic Modulation of Directional Solidification and Thermal Processing |
| YANG Minghui, LI Xingwu, SUN Chonghao, RUAN Ying |
| 图10 DS-TP条件下Monel K-500合金断口纵截面晶体取向及断裂前后样品的取向差角分布图 |
| Fig.10 Grain orientation distributions of longitudinal fracture section (Arrows show the grain boundaries formed during plastic deformation) (a1-c1) and misorientation distributions (a2-c2) of Monel K-500 alloys processed by synergetic modulation at growth rates of 5 μm/s (a1, a2), 50 μm/s (b1, b2), and 100 μm/s (c1, c2) (Insets show the misorientation distributions of Monel K-500 alloys before fracture) |
|