定向凝固与固态相变双联协控下Monel K-500合金的组织和力学性能 |
| 杨明辉, 李星吾, 孙崇昊, 阮莹 |
|
Microstructure and Mechanical Properties of Monel K-500 Alloy in Synergetic Modulation of Directional Solidification and Thermal Processing |
| YANG Minghui, LI Xingwu, SUN Chonghao, RUAN Ying |
| 图9 DS-TP条件下Monel K-500合金拉伸试样不同区域内局部取向差角分布图及其对应的极图 |
| Fig.9 Kernel average misorientation (KAM) distributions and pole figure (insets) in regions I (a1-c1), II (a2-c2), and III (a3-c3) in Fig.2a of the tensile specimen of Monel K-500 alloys processed by DS-TP at growth rates of 5 μm/s (a1-a3), 50 μm/s (b1-b3), and 100 μm/s (c1-c3) (The dotted circles in Figs.9b1-b3 show the projection of grain A on the pole figure) |
|