定向凝固与固态相变双联协控下Monel K-500合金的组织和力学性能 |
| 杨明辉, 李星吾, 孙崇昊, 阮莹 |
|
Microstructure and Mechanical Properties of Monel K-500 Alloy in Synergetic Modulation of Directional Solidification and Thermal Processing |
| YANG Minghui, LI Xingwu, SUN Chonghao, RUAN Ying |
| 图6 DS和DS-TP条件下Monel K-500合金微观组织TEM分析 |
| Fig.6 TEM analyses of Monel K-500 alloys processed by DS (a-c) and DS-TP (d-f) at growth rate of 5 μm/s (Insets in Fig.6e show the fast Fourier transform (FFT) patterns) (a, d) bright field (BF) and dark field (DF) images (b, e) high-resolution TEM (HRTEM) images (c, f) selected area electron diffraction (SAED) patterns |
|