综述:合金设计中物理模型与人工智能的集成与发展 |
| 王晨充, 徐伟 |
|
Overview: Integration and Development of Physical Models and Artificial Intelligence in Alloy Design |
| WANG Chenchong, XU Wei |
| 图5 热力学机制信息指导人工智能的合金设计范式[ |
| Fig.5 Paradigm of thermodynamic mechanism information-guided artificial intelligence for alloy design[ |
|