综述:合金设计中物理模型与人工智能的集成与发展 |
| 王晨充, 徐伟 |
|
Overview: Integration and Development of Physical Models and Artificial Intelligence in Alloy Design |
| WANG Chenchong, XU Wei |
| 图2 降维处理方法对模型准确性的量化影响[ |
| Fig.2 Quantitative effect of dimensionality reduction methods on model accuracy[ |
|