钨材料中缺陷的形成及演化规律
罗来马, 魏国庆, 刘祯, 朱晓勇, 吴玉程

Formation and Evolution of Defects in Tungsten Materials
LUO Laima, WEI Guoqing, LIU Zhen, ZHU Xiaoyong, WU Yucheng
图7 W中孪晶的形成与机理[127,128,135]
Fig.7 Formation and mechanism of twinning in W