钨材料中缺陷的形成及演化规律
罗来马, 魏国庆, 刘祯, 朱晓勇, 吴玉程

Formation and Evolution of Defects in Tungsten Materials
LUO Laima, WEI Guoqing, LIU Zhen, ZHU Xiaoyong, WU Yucheng
图5 W及钨合金拉伸性能汇总[61,64,88,91,92,97,100,102~106]
Fig.5 Summaries of tensile properties of W and tungsten alloys
(a) Nil ductility temperature (NDT)-ultimate tensile strength (UTS) summary (SPS—spark plasma sintering)[64,88,91,97,100,102-106]
(b) total elongation (TE)-UTS at 100 oC[61,64,88,91,92,100,102-104]