热轧加工工艺对快速降解Mg-Li合金力学性能及腐蚀行为的影响 |
| 庞梦瑶, 巫瑞智, 马晓春, 靳思远, 于哲, Boris Krit |
|
Effect of Hot Rolling Process on Mechanical Property and Corrosion Behavior of Rapidly Degrading Mg-Li Alloy |
| PANG Mengyao, WU Ruizhi, MA Xiaochun, JIN Siyuan, YU Zhe, Boris Krit |
| 图8 250 ℃下不同轧制变形量Mg-8Li-4Gd-1.5Ni合金在3%KCl溶液中浸泡后2和30 s后轧制方向-横向(RD-TD)平面上表面形貌的SEM像,及去除腐蚀产物后腐蚀表面形貌的SEM像 |
| Fig.8 RD-TD surface SEM images of rolled Mg-8Li-4Gd-1.5Ni alloy with deformations of 30% (a, e), 50% (b, f), 70% (c, g), and 90% (d, h) at 250 oC after soaking in 3%KCl solution for 2 s (a-d) and 30 s (e-h), and surface SEM images after removal of corrosion products after soaking in 3%KCl solution for 30 s (i-l) (TD—transverse direction) |
|