热轧加工工艺对快速降解Mg-Li合金力学性能及腐蚀行为的影响 |
| 庞梦瑶, 巫瑞智, 马晓春, 靳思远, 于哲, Boris Krit |
|
Effect of Hot Rolling Process on Mechanical Property and Corrosion Behavior of Rapidly Degrading Mg-Li Alloy |
| PANG Mengyao, WU Ruizhi, MA Xiaochun, JIN Siyuan, YU Zhe, Boris Krit |
| 图3 250 ℃下90%轧制变形量Mg-8Li-4Gd-1.5Ni合金的TEM像及EDS结果 |
| Fig.3 TEM images and corresponding EDS element maps of rolled Mg-8Li-4Gd-1.5Ni alloy with 90% deformation at 250 oC (a) GdNi3 (b) LPSO phase (Inset in Fig.3b show the selected area electron diffraction pattern) |
|