热轧加工工艺对快速降解Mg-Li合金力学性能及腐蚀行为的影响 |
| 庞梦瑶, 巫瑞智, 马晓春, 靳思远, 于哲, Boris Krit |
|
Effect of Hot Rolling Process on Mechanical Property and Corrosion Behavior of Rapidly Degrading Mg-Li Alloy |
| PANG Mengyao, WU Ruizhi, MA Xiaochun, JIN Siyuan, YU Zhe, Boris Krit |
| 图2 250 ℃下90%轧制变形量Mg-8Li-4Gd-1.5Ni合金的TEM像 |
| Fig.2 TEM images of rolled Mg-8Li-4Gd-1.5Ni alloy with 90% deformation at 250 oC (a) striated structure (b) recrystallized grain (c) dislocation |
|