Yb含量对Mg-Gd-Y-Zn-Zr合金微观组织与力学性能的影响 |
| 王升, 朱彦丞, 潘虎成, 李景仁, 曾志浩, 秦高梧 |
|
Effect of Yb Content on Microstructure and Mechanical Property of Mg-Gd-Y-Zn-Zr Alloy |
| WANG Sheng, ZHU Yancheng, PAN Hucheng, LI Jingren, ZENG Zhihao, QIN Gaowu |
| 图5 峰时效态GWZK-xYb合金的TEM表征 |
| Fig.5 TEM characterizations of the peak-aged GWZK-0Yb (a-c), GWZK-0.2Yb (d-f), and GWZK-0.5Yb (g-i) alloys (White lines Figs.5b, e, and h represent bending and twisting) |
|