AZ31镁合金双峰组织形成机制及其变形行为 |
| 周雯慧, 熊锦涛, 黄思程, 王鹏昊, 刘勇 |
|
Formation Mechanism and Deformation Behavior of AZ31 Magnesium Alloy Bimodal Structure |
| ZHOU Wenhui, XIONG Jintao, HUANG Sicheng, WANG Penghao, LIU Yong |
| 图2 AZ31镁合金的XRD谱、粗晶晶粒尺寸统计分析及粗晶显微组织OM和SEM像 |
| Fig.2 XRD spectra of alloys (a); statistical analysis of coarse grain size (b), OM image (c), and SEM image and EDS result (d) of coarse-grained AZ31 magnesium alloy |
|