高性能超高压镁合金研究进展 |
| 付辉, 孙勇, 邹国栋, 张帆, 杨许生, 张涛, 彭秋明 |
|
Research Progress in High-Performance Ultrahigh-Pressure Treated Magnesium Alloys |
| FU Hui, SUN Yong, ZOU Guodong, ZHANG Fan, YANG Xusheng, ZHANG Tao, PENG Qiuming |
| 图6 在3.5%NaCl (质量分数)溶液中浸泡不同时间后4 GPa-900 Mg-13Li样品表面的准原位SEM像[ |
| Fig.6 Near-in-situ SEM images of surfaces of 4 GPa-900 Mg-13Li sample immersed in 3.5%NaCl (mass fraction) solution for 5 min (a), 15 min (b), 30 min (c), 60 min (d), 90 min (e), and 120 min (f)[ |
|