高性能超高压镁合金研究进展 |
| 付辉, 孙勇, 邹国栋, 张帆, 杨许生, 张涛, 彭秋明 |
|
Research Progress in High-Performance Ultrahigh-Pressure Treated Magnesium Alloys |
| FU Hui, SUN Yong, ZOU Guodong, ZHANG Fan, YANG Xusheng, ZHANG Tao, PENG Qiuming |
| 图5 超高压处理对Mg-Al、Mg-Li及Mg-RE合金微观结构的影响 |
| Fig.5 Summary of effects of the UHP on the microstructure of the Mg-Al, Mg-Li, and Mg-RE alloys |
|