高性能超高压镁合金研究进展 |
| 付辉, 孙勇, 邹国栋, 张帆, 杨许生, 张涛, 彭秋明 |
|
Research Progress in High-Performance Ultrahigh-Pressure Treated Magnesium Alloys |
| FU Hui, SUN Yong, ZOU Guodong, ZHANG Fan, YANG Xusheng, ZHANG Tao, PENG Qiuming |
| 图4 Mg-Li基合金超高压力学性能比较[ |
| Fig.4 Comparisons of the yield strength and fracture ductility of UHPed Mg-Li-x alloys[ |
|