高性能超高压镁合金研究进展 |
| 付辉, 孙勇, 邹国栋, 张帆, 杨许生, 张涛, 彭秋明 |
|
Research Progress in High-Performance Ultrahigh-Pressure Treated Magnesium Alloys |
| FU Hui, SUN Yong, ZOU Guodong, ZHANG Fan, YANG Xusheng, ZHANG Tao, PENG Qiuming |
| 图2 不同状态Mg-30Al合金的OM像[ |
| Fig.2 OM images of Mg-30Al samples under different states[ (a) as-cast (b) SHP-2 GPa-800 (c) SHP-2 GPa-950 (d) SHP-4 GPa-1050 (e) SHP-4 GPa-1150 |
|