可降解镁基复合材料的制备及其在骨科领域的研究进展 |
| 欧阳思慧, 佘加, 陈先华, 潘复生 |
|
Preparation of Biodegradable Mg-Based Composites and Their Recent Advances in Orthopedic Applications |
| OUYANG Sihui, SHE Jia, CHEN Xianhua, PAN Fusheng |
| 图4 增材制造技术制备镁基复合材料实验装备示意图[ |
| Fig.4 Schematics of the selective laser melting process[ |
|