可充电镁电池负极材料及界面化学的研究进展 |
| 文恬恬, 岳继礼, 熊方宇, 袁媛, 黄光胜, 王敬丰, 潘复生 |
|
Research Progress on Anode Materials and Interfacial Chemistry for Rechargeable Magnesium Batteries |
| WEN Tiantian, YUE Jili, XIONG Fangyu, YUAN Yuan, HUANG Guangsheng, WANG Jingfeng, PAN Fusheng |
| 图9 负极固体电解质界面(SEI)膜改性:Mg2Ga5人工SEI膜[ |
| Fig.9 SEI fabricated anodes (a) Mg2Ga5 alloy-type layer[ (b) Ga5Mg2-Mg layer[ (c) Bi/MgCl2/PTHF (polytetrahydrofuran) SEI layer[ (d) schematic illustration of the MgMOF@Mg[ (e) zeolite-polymer SEI layer[ (f) phytic acid (PA) SEI layer[ (g) PA-Al SEI layer[ |
|