| 文恬恬, 岳继礼, 熊方宇, 袁媛, 黄光胜, 王敬丰, 潘复生 |
|
Research Progress on Anode Materials and Interfacial Chemistry for Rechargeable Magnesium Batteries |
| WEN Tiantian, YUE Jili, XIONG Fangyu, YUAN Yuan, HUANG Guangsheng, WANG Jingfeng, PAN Fusheng |
| 图2 Mg-Ga合金负极的代表性研究:Mg-Ga体系的固-液相变机制及长循环稳定性[ |
| Fig.2 Representative researches of Mg-Ga alloy anodes (a) solid-liquid phase transformation and long cycle-life of Mg-Ga system[ (b) morphologies of Ga confined by reduced graphene oxide (Ga@rGO) before and after charging process[ |
|