高容量镁基储氢合金材料研究与应用进展 |
| 邹建新, 张嘉祺, 赵颖燕, 林羲, 丁文江 |
|
Progress in the Research and Application of High-Capacity Mg-Based Hydrogen Storage Alloy Materials |
| ZOU Jianxin, ZHANG Jiaqi, ZHAO Yingyan, LIN Xi, DING Wenjiang |
| 图15 镁基固态储运氢技术在不同工业领域的应用 |