高容量镁基储氢合金材料研究与应用进展 |
| 邹建新, 张嘉祺, 赵颖燕, 林羲, 丁文江 |
|
Progress in the Research and Application of High-Capacity Mg-Based Hydrogen Storage Alloy Materials |
| ZOU Jianxin, ZHANG Jiaqi, ZHAO Yingyan, LIN Xi, DING Wenjiang |
| 图11 H2直接加热型镁基储氢罐与固体氧化物电解池(SOEC)和固体氧化物燃料电池(SOFC)耦合的潜在应用方案管道仪表流程图(PID)[ |
| Fig.11 PID diagram of potential applications for coupling hydrogen directly heated Mg-based hydrogen storage tanks (HST) with SOEC and SOFC[ |
|