高容量镁基储氢合金材料研究与应用进展 |
| 邹建新, 张嘉祺, 赵颖燕, 林羲, 丁文江 |
|
Progress in the Research and Application of High-Capacity Mg-Based Hydrogen Storage Alloy Materials |
| ZOU Jianxin, ZHANG Jiaqi, ZHAO Yingyan, LIN Xi, DING Wenjiang |
| 图10 导热油流速对镁镍合金储氢罐平均反应分数的影响及平均反应分数为0.8的横截面上反应分数的分布[ |
| Fig.10 Effect of heat transfer oil flow rate (uf) on average reaction fraction of magnesium-nickel alloys hydrogen storage tanks (a) and reaction fraction distributions on cross-section with average reaction fraction of 0.8 (b-f)[ |
|