镁合金电弧熔丝增材制造技术研究现状与展望 |
黄科, 李新志, 方学伟, 卢秉恒 |
State-of-the-Art Progress and Outlook in Wire Arc Additive Manufacturing of Magnesium Alloys |
HUANG Ke, LI Xinzhi, FANG Xuewei, LU Bingheng |
图19 层间强化辅助WAAM的设备[ |
Fig.19 Equipment for interlayer strengthening-assisted WAAM (a) interlayer hammering equipment[ (b) interlayer ultrasonic impact treatment[ (c) interlayer friction stir processing[ |
![]() |