镁合金电弧熔丝增材制造技术研究现状与展望 |
黄科, 李新志, 方学伟, 卢秉恒 |
State-of-the-Art Progress and Outlook in Wire Arc Additive Manufacturing of Magnesium Alloys |
HUANG Ke, LI Xinzhi, FANG Xuewei, LU Bingheng |
图12 本征热处理引起的WAAM制备WE43镁合金中的析出相演变[ |
Fig.12 Schematics showing the microstructure evolution with layer deposition during WAAM of WE43 alloy[ (a) the 1st layer (b) the 4th layer (c) the 15th layer (d) the top layer |
![]() |