镁合金电弧熔丝增材制造技术研究现状与展望
黄科, 李新志, 方学伟, 卢秉恒

State-of-the-Art Progress and Outlook in Wire Arc Additive Manufacturing of Magnesium Alloys
HUANG Ke, LI Xinzhi, FANG Xuewei, LU Bingheng
图9 AZ31镁合金在热轧态、钨极气体保护焊(GTAW)制备态和铸造态的晶粒尺寸和取向分布[35,38]
Fig.9 Grain sizes and crystallographic orientations of the AZ31 Mg alloy fabricated by hot-roll (a), GTAW (b, d), and semi-continuously cast (c)[35,38]