镁合金的多系滑移与塑性调控 |
| 曾小勤, 于铭迪, 王静雅 |
|
Multi-Slips and Ductility Regulation of Magnesium Alloys |
| ZENG Xiaoqin, YU Mingdi, WANG Jingya |
| 图3 基于微柱压缩方法测定的Mg-Zn-Ca合金沿a轴压缩的应力-应变曲线;从前、后视角分析微柱表面滑移迹线的SEM像及晶体学取向示意图[ |
| Fig.3 Engineering stress-strain curves of Mg-Zn-Ca alloys loading along the a-axis based on the micropillar compression method (D: [10 |
|