中锰钢奥氏体中化学界面变形行为的晶体塑性研究 |
|||||||||||||||
| 贾春妮, 刘腾远, 郑成武, 王培, 李殿中 | |||||||||||||||
|
Micro-Deformation Behavior of Austenite Containing Chemical Boundary in a Medium Mn Steel: A Crystal Plasticity Modeling |
|||||||||||||||
| JIA Chunni, LIU Tengyuan, ZHENG Chengwu, WANG Pei, LI Dianzhong | |||||||||||||||
| 表5 奥氏体内部Mn化学界面两侧的微区应力及应变差统计值 |
|||||||||||||||
| Table 5 Statistics of the difference value of microzone strain and stress across the chemical boundary |
|||||||||||||||
|
|||||||||||||||