中锰钢奥氏体中化学界面变形行为的晶体塑性研究 |
| 贾春妮, 刘腾远, 郑成武, 王培, 李殿中 |
|
Micro-Deformation Behavior of Austenite Containing Chemical Boundary in a Medium Mn Steel: A Crystal Plasticity Modeling |
| JIA Chunni, LIU Tengyuan, ZHENG Chengwu, WANG Pei, LI Dianzhong |
| 图6 应变为0.025时沿图4b和5b中L1-L |
| Fig.6 Microzone stress (a, c) and microzone strain (b, d) distributions along the lines L1-L |
|