中锰钢奥氏体中化学界面变形行为的晶体塑性研究 |
| 贾春妮, 刘腾远, 郑成武, 王培, 李殿中 |
|
Micro-Deformation Behavior of Austenite Containing Chemical Boundary in a Medium Mn Steel: A Crystal Plasticity Modeling |
| JIA Chunni, LIU Tengyuan, ZHENG Chengwu, WANG Pei, LI Dianzhong |
| 图5 奥氏体内部化学界面附近的微区应力演化 |
| Fig.5 Simulated microzone stress distributions across the chemical boundary within an austenite grain at strains of 0.025 (a), 0.05 (b), 0.075 (c), and 0.1 (d) |
|