表3 1100 ℃元素扩散模型拟合参数
|
Table 3 Fitting parameters of the element diffusion model at 1100 oC
|
|
| Reduction rate | Element | A | B1 | B2 | α | β | D1 | D2 |
|---|
| 20% | Fe | 0.808 | 0.161 | 0.145 | 0.328 | 1.921 | 2.171 | 2.000 | | Cr | 0.094 | -0.102 | -0.086 | 0.591 | 1.050 | 3.150 | 2.452 | | Ni | 0.041 | -0.043 | -0.039 | -2.304 | 2.444 | 1.353 | 0.905 | | 40% | Fe | 0.801 | 0.153 | 0.154 | 1.014 | 1.386 | 1.509 | 1.204 | | Cr | 0.087 | -0.109 | -0.077 | 1.185 | 1.554 | 4.085 | 1.679 | | Ni | 0.043 | -0.042 | -0.042 | -0.252 | -1.445 | 2.827 | 6.530 | | 60% | Fe | 0.801 | 0.156 | 0.153 | 1.308 | 0.862 | 2.005 | 3.193 | | Cr | 0.096 | -0.099 | -0.085 | 2.952 | 1.443 | 0.859 | 3.311 | | Ni | 0.042 | -0.045 | -0.042 | 0.790 | -0.321 | 1.268 | 3.816 |
|
|
|