不锈钢复合钢筋近界面微观组织演变及元素扩散动力学 |
| 郭星星, 帅美荣, 楚志兵, 李玉贵, 谢广明 |
|
Microstructure Evolution Near Interface and the Element Diffusion Dynamics of the Composite Stainless Steel Rebar |
| GUO Xingxing, SHUAI Meirong, CHU Zhibing, LI Yugui, XIE Guangming |
| 图2 不锈钢复合钢筋在1000 ℃时测量区域示意图(40%压下率)和不同压下率时复合界面显微组织的SEM像 |
| Fig.2 Schematic of the measurement zone (a) and SEM images of the composite interface of composite stainless steel rebar with reduction rates of 20% (b), 40% (c), and 60% (d) at 1000 oC (Black dash lines in Figs.2b-d show the boundaries of carburized layer, and red dash lines show twin boundaries. The schematic of the measurement zone is illustrated by an example with reduction rate of 40%) |
|