聚变增殖包层用低活化9Cr-ODS钢的室温低周疲劳行为 |
| 王旗涛, 李艳芬, 张家榕, 李尧志, 付海阳, 李新乐, 严伟, 单以银 |
|
Low Cycle Fatigue Behavior of 9Cr-ODS Steel as a Fusion Blanket Structural Material at Room Temperature |
| WANG Qitao, LI Yanfen, ZHANG Jiarong, LI Yaozhi, FU Haiyang, LI Xinle, YAN Wei, SHAN Yiyin |
| 图10 9Cr-ODS、中国低活化马氏体(CLAM)钢[ |
| Fig.10 Fatigue response curves of 9Cr-ODS, China low activation martensitic (CLAM)[ |
|