静水压力和拉伸应力交互作用下Ni-Cr-Mo-V钢在3.5%NaCl溶液中的应力腐蚀行为 |
| 宋昱杉, 刘叡, 崔宇, 刘莉, 王福会 |
|
Stress Corrosion Behavior of Ni-Cr-Mo-V Steel in 3.5%NaCl Solution Under the Interaction of Hydrostatic Pressure and Tensile Stress |
| SONG Yushan, LIU Rui, CUI Yu, LIU Li, WANG Fuhui |
| 图15 Ni-Cr-Mo-V钢经过应变速率为1 × 10-6的SSRT实验后的侧面形貌放大图 |
| Fig.15 Magnified side surface morphologies of Ni-Cr-Mo-V steel after SSRT test at 1 × 10-6 s-1 in air (a), and 0.1 MPa (b) and 20 MPa (c) in 3.5%NaCl solution |
|