静水压力和拉伸应力交互作用下Ni-Cr-Mo-V钢在3.5%NaCl溶液中的应力腐蚀行为 |
| 宋昱杉, 刘叡, 崔宇, 刘莉, 王福会 |
|
Stress Corrosion Behavior of Ni-Cr-Mo-V Steel in 3.5%NaCl Solution Under the Interaction of Hydrostatic Pressure and Tensile Stress |
| SONG Yushan, LIU Rui, CUI Yu, LIU Li, WANG Fuhui |
| 图14 Ni-Cr-Mo-V钢在不同条件下的线性极化曲线、线性极化电阻和腐蚀电流密度 |
| Fig.14 Linear polarization curves (a-d), linear-polarization resistances (Rp) (e), and corrosion current densities (f) of Ni-Cr-Mo-V steel as a function of immersion time in 3.5%NaCl solution under different conditions |
|