静水压力和拉伸应力交互作用下Ni-Cr-Mo-V钢在3.5%NaCl溶液中的应力腐蚀行为 |
| 宋昱杉, 刘叡, 崔宇, 刘莉, 王福会 |
|
Stress Corrosion Behavior of Ni-Cr-Mo-V Steel in 3.5%NaCl Solution Under the Interaction of Hydrostatic Pressure and Tensile Stress |
| SONG Yushan, LIU Rui, CUI Yu, LIU Li, WANG Fuhui |
| 图4 Ni-Cr-Mo-V钢在不同环境中进行SSRT实验后得到的应变-应力曲线、断裂伸长率和断裂强度 |
| Fig.4 Mechanical properties of Ni-Cr-Mo-V steel after SSRT test under different conditions (a) strain-stress curve (b) fracture strain (c) fracture strength |
|