南极大气环境下Q460和Q690 低合金钢的腐蚀行为
闫茂鑫, 李杰, 王哲超, 姚旭, 胡秉晨, 葛峰, 崔中雨, 王昕, 崔洪芝

Atmospheric Corrosion Behavior of Q460 and Q690 Low Alloy Steels in Antarctic Environment
YAN Maoxin, LI Jie, WANG Zhechao, YAO Xu, HU Bingchen, GE Feng, CUI Zhongyu, WANG Xin, CUI Hongzhi
图10 低合金钢Q460和Q690暴露于南极大气环境形成的腐蚀产物的物相分布
Fig.10 Phase distributions of the corrosion products (see in Fig.6) formed on Q460 (a) and Q690 (b) low alloy steels (A, G, L, and M represent akaganeite (β-FeOOH), goethite (α-FeOOH), lepidocrocite (γ-FeOOH), and megnetite/meghemite (Fe3O4/γ-Fe2O3), respectively)