南极大气环境下Q460和Q690 低合金钢的腐蚀行为 |
闫茂鑫, 李杰, 王哲超, 姚旭, 胡秉晨, 葛峰, 崔中雨, 王昕, 崔洪芝 |
Atmospheric Corrosion Behavior of Q460 and Q690 Low Alloy Steels in Antarctic Environment |
YAN Maoxin, LI Jie, WANG Zhechao, YAO Xu, HU Bingchen, GE Feng, CUI Zhongyu, WANG Xin, CUI Hongzhi |
图7 南极大气环境下Q460和Q690低合金钢暴露不同时间的表面腐蚀形貌 |
Fig.7 Surface morphologies and 3D topographies of Q460 (a1-a4, c1-c4) and Q690 (b1-b4, d1-d4) low alloy steels exposed to Antarctic atmosphere for 1 month (a1-a4, b1-b4) and 12 months (c1-c4, d1-d4) (a1-d1, a2-d2) skyward (a3-d3, d4-d4) groundward |
![]() |