南极大气环境下Q460和Q690 低合金钢的腐蚀行为
闫茂鑫, 李杰, 王哲超, 姚旭, 胡秉晨, 葛峰, 崔中雨, 王昕, 崔洪芝

Atmospheric Corrosion Behavior of Q460 and Q690 Low Alloy Steels in Antarctic Environment
YAN Maoxin, LI Jie, WANG Zhechao, YAO Xu, HU Bingchen, GE Feng, CUI Zhongyu, WANG Xin, CUI Hongzhi
图1 本实验中的南极中山站暴露地点
Fig.1 Exposure site in Zhongshan station in Antarctic continent