Zn-2.0Al-1.5Mg镀层在模拟海洋大气中的腐蚀行为
|
|
顾天真, 刘雨薇, 彭灿, 张鹏, 王振尧, 汪川, 马成, 曹宏玮
|
Corrosion Behavior of Zn-2.0Al-1.5Mg Coatings in Simulated Marine Atmosphere
|
|
GU Tianzhen, LIU Yuwei, PENG Can, ZHANG Peng, WANG Zhenyao, WANG Chuan, MA Cheng, CAO Hongwei
|
|
表1 EIS参数拟合结果
|
Table 1 Impedance parameters of Zn-2.0Al-1.5Mg coating after being fitted
|
|
Time h | Rs Ω·cm2 | Qr | Rr Ω·cm2 | Qdl | Rct Ω·cm2 | Chi-squared | Rp (= Rr + Rct) Ω·cm2 |
|---|
yr Ω-1·cm-2·S | nr | ydl Ω-1·cm-2·S | ndl |
|---|
| 0 | 4.33 × 101 | 1.30 × 10-5 | 6.56 × 10-1 | 7.20 × 103 | 6.26 × 10-5 | 9.71 × 10-1 | 6.44 × 103 | 9.29 × 10-3 | 1.36 × 104 | | 168 | 5.05 × 101 | 1.48 × 10-5 | 6.81 × 10-1 | 8.26 × 102 | 2.05 × 10-3 | 5.23 × 10-1 | 8.94 × 102 | 5.87 × 10-3 | 1.72 × 103 | | 336 | 8.53 × 10-4 | 2.02 × 10-5 | 4.65 × 10-1 | 2.31 × 102 | 6.74 × 10-7 | 9.60 × 10-1 | 2.87 × 104 | 2.39 × 10-2 | 2.89 × 104 | | 504 | 2.51 × 101 | 1.07 × 10-5 | 6.95 × 10-1 | 2.84 × 103 | 1.19 × 10-4 | 6.36 × 10-1 | 5.52 × 103 | 7.11 × 10-3 | 8.36 × 103 | | 672 | 4.21 × 10-3 | 3.03 × 10-5 | 4.58 × 10-1 | 7.89 × 102 | 2.09 × 10-7 | 1.00 × 100 | 6.33 × 103 | 6.47 × 10-3 | 7.12 × 103 | | 840 | 3.07 × 101 | 1.77 × 10-5 | 5.50 × 10-1 | 5.52 × 103 | 4.13 × 10-4 | 8.78 × 10-1 | 4.59 × 103 | 4.34 × 10-2 | 1.01 × 104 | | 1848 | 3.14 × 10-23 | 1.51 × 10-3 | 8.38 × 10-2 | 4.70 × 10-19 | 4.63 × 10-7 | 7.34 × 10-1 | 5.95 × 102 | 7.36 × 10-4 | 5.95 × 102 |
|
|
|