Zn-2.0Al-1.5Mg镀层在模拟海洋大气中的腐蚀行为
顾天真, 刘雨薇, 彭灿, 张鹏, 王振尧, 汪川, 马成, 曹宏玮

Corrosion Behavior of Zn-2.0Al-1.5Mg Coatings in Simulated Marine Atmosphere
GU Tianzhen, LIU Yuwei, PENG Can, ZHANG Peng, WANG Zhenyao, WANG Chuan, MA Cheng, CAO Hongwei
图12 NaCl溶液中Cl-的平衡浓度(CCl-)随相对湿度的变化[37]
Fig.12 Variations of the equilibrium concentration of chloride solution (CCl-) of NaCl solution with different relative humidities[37]