Zn-2.0Al-1.5Mg镀层在模拟海洋大气中的腐蚀行为 |
| 顾天真, 刘雨薇, 彭灿, 张鹏, 王振尧, 汪川, 马成, 曹宏玮 |
|
Corrosion Behavior of Zn-2.0Al-1.5Mg Coatings in Simulated Marine Atmosphere |
| GU Tianzhen, LIU Yuwei, PENG Can, ZHANG Peng, WANG Zhenyao, WANG Chuan, MA Cheng, CAO Hongwei |
| 图6 Zn-2.0Al-1.5Mg镀层在模拟海洋大气环境中腐蚀1848 h后截面形貌的SEM像和EDS元素分布 |
| Fig.6 SEM image and corresponding EDS mappings of elements of Zn-2.0Al-1.5Mg coating in the simulated marine atmosphere at 1848 h |
|