Ti6246钛合金 β → α 相变中晶界 α 相生长行为及其对微织构的影响 |
| 齐敏, 王倩, 马英杰, 曹贺萌, 黄森森, 雷家峰, 杨锐 |
|
Growth Behavior of Grain Boundary α Phase and Its Effect on the Microtexture During β → α Phase Transformation in Ti6246 Titanium Alloys |
| QI Min, WANG Qian, MA Yingjie, CAO Hemeng, HUANG Sensen, LEI Jiafeng, YANG Riu |
| 图8 Ti6246合金由β单相区炉冷至两相区不同温度后α相的EBSD分析 |
| Fig.8 EBSD analyses of the α phase in the Ti6246 alloy after furnace cooling from β phase field to 920 oC (a), 880 oC (b), and 840 oC (c) (The area enclosed by dashed line in Fig.8c indicates that the β phase has not yet transformed to α phase) |
|