粉末粒度对钛合金闭式叶轮成形的影响 |
| 尚学文, 崔潇潇, 徐磊, 卢正冠 |
|
Effect of Powder Particle Size on Forming Titanium Alloy Shrouded Impeller |
| SHANG Xuewen, CUI Xiaoxiao, XU Lei, LU Zhengguan |
| 图10 有限元模拟叶轮尺寸收缩前后对比 |
| Fig.10 Finite element method (FEM) simulation of impeller sizes before (a) and after (b) shrinkage |
|