粉末粒度对钛合金闭式叶轮成形的影响 |
| 尚学文, 崔潇潇, 徐磊, 卢正冠 |
|
Effect of Powder Particle Size on Forming Titanium Alloy Shrouded Impeller |
| SHANG Xuewen, CUI Xiaoxiao, XU Lei, LU Zhengguan |
| 图5 叶轮本体取样的低温(77 K)力学性能 |
| Fig.5 Tensile properties of impellers at 77 K (RA—reduction of area) (a) different positions of the same impeller (2#) (b) comprehensive comparison of different impellers |
|