FGH96合金静态再结晶过程的显微组织演化 |
| 彭子超, 罗俊鹏, 赵宇, 周磊, 王旭青, 邹金文 |
|
Evolution of Microstrucutre During Static Recrystallization in FGH96 Superalloy |
| PENG Zichao, LUO Junpeng, ZHAO Yu, ZHOU Lei, WANG Xuqing, ZOU Jinwen |
| 图1 不同状态FGH96合金试样显微组织的OM像 |
| Fig.1 OM images of FGH96 superalloy with different solution temperatures (a) forged (b) 1100 oC (c) 1120 oC (d) 1140 oC (e) 1160 oC (f) 1180 oC (g) 1220 oC (h) 1260 oC |
|