一种 γ'/γ'' 相强化镍基高温合金的蠕变行为 |
| 周生玉, 胡明昊, 李冲, 丁海民, 郭乾应, 刘永长 |
|
Creep Behavior of a Ni-Based Superalloy with Strengthening of γ' and γ'' Phases |
| ZHOU Shengyu, HU Minghao, LI Chong, DING Haimin, GUO Qianying, LIU Yongchang |
| 图8 蠕变试样断口附近的轴向变形组织的SEM像 |
| Fig.8 SEM images of longitudinal sections near the fractures of HDA-7 (a), HDA-8 (b), and HDA-9 (c) |
|